No not really. Around 190c, but have tried both lower and higher. I printed a big lampfoot, that did change colour in the beginning. It sits in...
How come so many say e3d have 0 ooze (v5)?? Mine snivles like a dog with a cold.. I think i have got a real "monday example".. = troubles,...
I drilled the heatbreak ( is still have an original to revert to) to 3.2mm instead of the original 3.1, now it seems no more jams. I think my...
The UV changing filament only works for a week or two. After that it won't react to the sun anymore. Only printed objects that is. On the spool...
I am getting tired of this now, i have jamming problems again. Especially with ABS. Nylon is still printing ok, but that is because nylon is...
I got the new v6 nozzles and they print really good now (without drilling ;). I have printed a lot of different nylons, PLA and Ninjaflex, not had...
Josh: I have done a lot of testing lately. I had success printing ABS after the drillout of my 0.6 nozzle, but still a lot of sticking with NYLON...
I have been really successful in printing a lot now with drilled 0.6 nozzle. My new favourite material to print is nylon. I have been using...
Grr.... the 0.25 nozzle blew open after 20minutes, it seems i drilled too much so the walls got weakened :( Getting a bit tired of this bull......
Makerbot PLA did i print at 190c with original hotend, on e3d i have tried up to 220. The 220 i wrote above is for the PS1 ABS, but have tried up...
I should add that extruder is calibrated and also PID. Temp in range of one degree.
Sure. I also handdrilled with fingers, but as Mike i was also too eager...this was before i got the heat/insert PLA/cool and pull method working...
I am actually having some success finally. I drilled the .6 nozzle to 0.8mm boredepth but still had some problems, so i tried another tip from...