Separate names with a comma.
I'm using arctic MX4 on the heatbreak to heatsink thread. I can't find anything saying I shouldn't or any spec at all for max temp for MX4 - I...
I have pretty much the same problem. Only difference is that it happens 4-10 hours into an 18 hour print. Titan Aeros jam a lot, that has been my...
I used a hardened nozzle for ages with carbon filled PLA but found it prone to jams. The plated copper nozzle has not jammed yet and I have...
I have read everything I can find on using XT-CF20 on this forum and I'm still not getting good results. I've been printing with carbon filled PLA...
The warranty says that the non-stick coating is not covered by the warranty - I would assume that means the nanoweb coating - it does not say...
OK, so it is the same plating as the copper nozzle. So what is the expected lifetime of the plating on the nozzle X in terms of printing typical...
90% of my printing is carbon fibre filled, usually PLA. The regular hardened nozzle is a bit prone to clogs. I've been printing with the plated...