Heatbreak not poslished all the way.

Discussion in 'E3D-v6 and Lite6' started by Thesecky, Nov 8, 2017.

Tags:
  1. Thesecky

    Thesecky Member

    Joined:
    Nov 8, 2017
    Messages:
    5
    Likes Received:
    0
    Hi, today i inspeacted my new heatbreak i got with my e3d, and i notice that the 2mm part isnt polished all the way. Only the hot zone part is, and the transition zone is the same as my clones, you can see the drilling marks. Are the heatbreaks only polished up to the end of the hot zone? Thanks for your time.
     
  2. Antoine

    Antoine Well-Known Member
    Staff Member

    Joined:
    Apr 3, 2017
    Messages:
    47
    Likes Received:
    10
    Could you possibly send a picture of what you are seeing? This might have slipped through our QC but it is difficult to tell from your description. In any case, excessive tooling marks are not acceptable.
     
  3. Thesecky

    Thesecky Member

    Joined:
    Nov 8, 2017
    Messages:
    5
    Likes Received:
    0
    I really cannot send you a picture since my cameras cant shoot is such focus for so small datails. But i found this photo online, the red circle that i circled is the place where the throat is polished, the rest looks rough on mine.
     