Help With Titan Aero Clog

Discussion in 'Titan' started by ewr2san, Nov 29, 2018.

  1. ewr2san

    ewr2san Member

    Joined:
    Nov 29, 2018
    Messages:
    2
    Likes Received:
    0
    Hello,

    I've checked all the following:
    1. Retraction is set to 0.4
    2. Temps are all good. 200-220c.
    3. Have done 3 cold pulls including atomic.

    To me it looks like I have a partial clog at the top of the Heatbrake or in the coldzone. How do I clear it?

    Here's what my pulls look like:
    [​IMG]
     
  2. ewr2san

    ewr2san Member

    Joined:
    Nov 29, 2018
    Messages:
    2
    Likes Received:
    0
    The picture posted "upside down" The top is the bottom end of the filament. The Filament narrows about 35mm from the nozzle area.


     
  3. Old_Tafr

    Old_Tafr Well-Known Member

    Joined:
    Mar 7, 2016
    Messages:
    698
    Likes Received:
    90
    If you can remove clogging with a cold-pull then I guess the only way is to dismantle and rebuild.
     